| CPC C08L 95/00 (2013.01) [C08L 91/06 (2013.01); D06N 5/003 (2013.01); C08L 23/02 (2013.01); C08L 53/02 (2013.01); C08L 2555/86 (2013.01)] |
| AS A RESULT OF REEXAMINATION, IT HAS BEEN DETERMINED THAT: |
| Claims 1-19 are cancelled. |
|
non-oxidized base asphalt; and
a low MW polyolefin present in an amount of no more than about 1.8 wt % based on the total weight of the asphalt composition, wherein said asphalt composition has a softening point from about 87.8 to about 160 °C (about 190 to about 320°F), and a penetration of greater than about 12 deci-millimeters (dmm, or 0.1 mm) @ 25 °C, and wherein the low MW polyolefin has a crystallinity of from about 30 to about 100 percent (%).
|