| US 7,543,733 B2 | ||
| Method of protecting against corrosion at high temperature | ||
| Sophie Wastiaux, Aulnay Sous Bois (France); and Michel Poteau, Dammartin En Goele (France) | ||
| Assigned to L'Air Liquide, Societe Anonyme A Directoire et Conseil de Surveillance pour l'Etude et l'Exploitation des Procedes Georges Claude, Paris (France) | ||
| Filed on Jun. 25, 2003, as Appl. No. 10/603,530. | ||
| Claims priority of application No. 03 03238 (FR), filed on Mar. 17, 2003. | ||
| Prior Publication US 2005/0173495 A1, Aug. 11, 2005 | ||
| Int. Cl. B21D 39/04 (2006.01); B23K 1/00 (2006.01) | ||
| U.S. Cl. 228—128 [228/126; 228/127; 228/131; 228/182; 228/183; 228/184; 228/189; 285/55; 285/288.1; 285/288.6] | 7 Claims |

| 1. A method for protecting a tubular junction, comprising:
providing a first tubular and a second tubular, each tubular having an outer surface and an interior surface for the passage
of fluid;
placing a protective surface finish on an interior of the tubulars;
providing a joining tubular having a surface finish on an interior thereof;
connecting the joining tubular between the first and second tubulars to create a junction, the junction only including the
joining tubular and an end of each of the first and second tubulars and having a continuous surface finish on an interior
surface thereof; and
welding the joining tubular to the first and second tubulars in a manner whereby the continuous surface finish remains on
the interior surface of the junction along a non-welded portion between the joining tubular and the end of each of the first
and second tubulars.
|