| US 7,538,988 B2 | ||
| Method and apparatus having improved magnetic read head sensors | ||
| Jinshan Li, San Jose, Calif. (US); and Alexander M. Zeltser, San Jose, Calif. (US) | ||
| Assigned to Hitachi Global Storage Technologies Netherlands B.V., Amsterdam (Netherlands) | ||
| Filed on Sep. 30, 2004, as Appl. No. 10/955,396. | ||
| Prior Publication US 2006/0067012 A1, Mar. 30, 2006 | ||
| Int. Cl. G11B 5/127 (2006.01) | ||
| U.S. Cl. 360—324.11 | 17 Claims |

| 1. An synthetic or AP pinned layer in a GMR stack, comprising a cobalt-iron ternary alloy layer, wherein a third constituent of the cobalt-iron ternary alloy layer is selected from the group consisting of vanadium, chromium, molybdenum and tungsten , wherein the amount of the third constituent of the cobalt-iron ternary alloy ranges from about 0.5 to about 7.0 atomic percent and the iron in the cobalt-iron ternary alloy ranges from about 10 to about 55 atomic percent, wherein a percentage of the third constituent of the cobalt-iron ternary alloy layer is selected to provide a magnetostriction ranging from about 2×105 to about 4×105. |