| US 7,523,846 B2 | ||
| Scribing method, cutter wheel, scribing device using the cutter wheel, and cutter wheel manufacturing device for manufacturing the cutter wheel | ||
| Kiyoshi Takamatsu, Osaka (Japan); Kazuya Maekawa, Osaka (Japan); and Noriyuki Ogasawara, Osaka (Japan) | ||
| Assigned to Mitsuboshi Diamond Industrial Co., Ltd., Osaka (Japan) | ||
| Appl. No. 10/468,754 PCT Filed Mar. 15, 2002, PCT No. PCT/JP02/02522 § 371(c)(1), (2), (4) Date Apr. 07, 2004, PCT Pub. No. WO02/074707, PCT Pub. Date Sep. 26, 2002. |
||
| Claims priority of application No. 2001-76082 (JP), filed on Mar. 16, 2001. | ||
| Prior Publication US 2004/0155085 A1, Aug. 12, 2004 | ||
| Int. Cl. B26F 3/00 (2006.01); B31B 1/25 (2006.01) | ||
| U.S. Cl. 225—2 [225/1; 225/103; 83/866; 83/880] | 17 Claims |

| 1. A scribing method using a brittle material separation disk-shaped wheel having a central portion in a thickness direction
protruding in a circumferential direction so as to form a blade edge at an edge line portion of the wheel,
wherein the edge line portion of the disk-shaped wheel comprises at least one region (A) and at least one region (B),
region (A) is a region where a plurality of grooves having a predetermined shape are formed in the edge line portion with
a predetermined pitch, while region (B) is a region where grooves are not formed in the edge line portion, and
in the brittle material separation disk-shaped wheel the ratio of a length of a region occupied by the plurality of grooves
with respect to an entire perimeter of the edge line portion is equal to or smaller than ¾,
comprising performing scribing along a scribe line on a brittle material using the wheel to form a vertical crack in the brittle
material that varies periodically in depth along the scribe line without extending through the brittle material,
wherein the scribe line is formed on the glass substrate, and the vertical crack is extended by applying a force to widen
horizontally the vertical crack, the vertical crack being formed along the vertical direction of the scribe line on the glass
substrate; and
wherein the depth of the vertical crack is periodically varied according to the depth of the plurality of grooves under a
constant load.
|