| US 7,514,144 B2 | ||
| Tablet, process for producing the same, and molded article obtained therefrom | ||
| Hideyuki Umetsu, Nagoya (Japan); Fumie Shinoda, Nagoya (Japan); and Yoshiki Makabe, Nagoya (Japan) | ||
| Assigned to Toray Industries, Inc., (Japan) | ||
| Appl. No. 10/432,390 PCT Filed May 21, 2002, PCT No. PCT/JP02/04911 § 371(c)(1), (2), (4) Date May 21, 2003, PCT Pub. No. WO02/094529, PCT Pub. Date Nov. 28, 2002. |
||
| Claims priority of application No. 2001-156063 (JP), filed on May 24, 2001; application No. 2001-318757 (JP), filed on Oct. 16, 2001; application No. 2001-318759 (JP), filed on Oct. 16, 2001; and application No. 2001-318762 (JP), filed on Oct. 16, 2001. | ||
| Prior Publication US 2005/0098916 A1, May 12, 2005 | ||
| Int. Cl. B32B 5/66 (2006.01) | ||
| U.S. Cl. 428—402 [428/403; 428/404; 428/405; 428/406; 428/407; 428/328; 427/212; 427/384] | 11 Claims |
| 1. A tablet comprising a thermoplastic resin and a filler, having a compositional ratio of 1 to 50% by volume of the thermoplastic resin and 50 to 99% by volume of the filler, based on the thermoplastic resin and the filler, and 0.1 to 30 parts by weight of at least one of a substance selected from the group consisting of a substance (X) that changes from solid into liquid or vapor at a temperature falling between 25 and 250° C., a liquid organic compound of which the viscosity at 25° C. falls between 1 and 5000 mPa·s and a phosphate, based on 100 parts by weight of the thermoplastic resin and the filler. |