| US 7,498,079 B1 | ||
| Thermally stable polytetrafluoroethylene fiber and method of making same | ||
| Mike Donckers, Decatur, Ala. (US) | ||
| Assigned to Toray Fluorofibers (America), Inc., Decatur, Ala. (US) | ||
| Filed on Jun. 14, 2007, as Appl. No. 11/763,249. | ||
| Claims priority of provisional application 60/943759, filed on Jun. 13, 2007. | ||
| Int. Cl. D02G 3/00 (2006.01) | ||
| U.S. Cl. 428—364 [426/394; 426/421] | 27 Claims |

| 1. A polytetrafluoroethylene fiber exhibiting less than 9% shrinkage when subjected to a temperature of 300 degrees Celsius for 30 minutes wherein the polytetrafluoroethylene fiber is a dispersion spun fiber. |